3D deformation modeling of CrAlN coated tool steel compound during nanoindentation
Surface and Coatings Technology(2023)
摘要
The finite element method (FEM) nanoindentation simulations of nitride hard coatings are either focused on the coating only or contain an axisymmetric model of the coated compound with isotropic material behavior. Moreover, the material model parameters are optimized at only one particular indentation load. The current work aims to develop a 3D FEM model for studying deformation behavior of a CrAlN PVD coated HS6-5-2C tool steel compound during nanoindentation at varying indentation loads. A machine learning (ML)-based algorithm was used to characterize the coating microstructure. This information allowed to set up a 3D FEM model containing a digital clone of the compound microstructure along with the local orientations of the grains embedded into a larger elastically modelled frame. The material model parameters such as Young's modulus E, yield stress Y, strain hardening coefficient B and strain hardening exponent n for coating, interlayer and substrate were determined by fitting the simulated force-displacement curves to the experimental ones through an iterative optimization approach at four different indentation loads. An overall good agreement between the simulated and experimental force-displacement curves along with physically reasonable material model parameters was achieved. The obtained yield stress of CrAlN coating was comparable to ceramics. Moreover, elastic-plastic deformation in interlayer and elastic deformation in substrate at indentation depth below 10 % of the coating thickness was observed. This necessitates the interlayer and substrate consideration for FEM nanoindentation simulations of PVD coated compounds as in the present study. Therefore, the used modeling approach, based on orthotropic elastic material law for the coating combined with 3D digital clone of the compound microstructure, was successfully implemented and validated for low as well as high indentation loads.
更多查看译文
关键词
PVD,CrAlN,FEM simulation,Microstructure,Nanoindentation,Deformation
AI 理解论文
溯源树
样例
![](https://originalfileserver.aminer.cn/sys/aminer/pubs/mrt_preview.jpeg)
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要