Manganese oxide-supported palygorskite (MnOx/PG) catalysts are considered highly efficient for low-temperature SCR of NOx. However, the MnOx/PG catalyst tends to be poisoned by SO2. The effect of SO2 on activity of the SO2-pretreated poisoning catalysts under ammonia-free conditions was explored. It was determined that the MnOx/PG catalyst tends to be considerably deactivated by SO2 in the absence of ammonia and that water-washed regeneration can completely recover activity of the deactivated catalyst. Based on these results and characterizations of the catalysts, a reasonable mechanism for the deactivation of MnOx/PG catalyst by SO2 was proposed in this study. SO2 easily oxidized to SO3 on the surface of the catalyst, leading to the formation of polysulfuric acid, wrapping of the active component and blocking the micropores. The deactivation of the MnOx/PG catalyst is initially caused by the formation of polysulfuric rather than the deposition of ammonia sulfate, which occurs later.
更多
查看译文
关键词
low-temperature SCR, MnOx, <p>MnOx/PG catalyst</p>, SO2-pretreated poisoning, water-washed regeneration
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要