Experiments and numerical simulations for the mechanical properties of Ni-based superalloys fabricated by laser melting deposition
Optics & Laser Technology(2021)
摘要
•Crack-free Hastelloy X multilayer samples were prepared by laser melting deposition.•The mechanical properties of Hastelloy X was analyzed by finite element simulation.•The J-C constitutive model was constructed to predict the stretching behavior.•The microhardness of LMD Hastelloy X is 1.3 times that of wrought Hastelloy X.
更多查看译文
关键词
Laser melting deposition (LMD),Johnson-Cook (J-C) model,Finite element analysis,Mechanical properties