Multiscale Digital Twin For Particle Breakage In Milling: From Nanoindentation To Population Balance Model
POWDER TECHNOLOGY(2021)
摘要
A multiscale modelling approach to integrate resultful information of particle breakage at distinct scales is presented for quantitative prediction of a milling process. The nanoindentation test of zeolite particles is carried out to provide the deterministic value of mechanical properties, prior to which the Hertz based contact theory is described. The impact pin milling test is made to measure the particle size distribution subject to three rotary speeds. The population balance model composed of selection function and breakage function is developed to predict the varying milling operations based on successful model validation. With the hybrid of theoretical, experimental and numerical avenues, a conceptual multiscale modelling roadmap with complementary strength is proposed. The best available information spanning distinct scales is scoped where the interaction of physical twin and digital twin is highlighted. Global system analysis of the key parameters provides projected confidence in milling performance beyond the existing experimental space.(c) 2021 Elsevier B.V. All rights reserved.
更多查看译文
关键词
Multiscale milling, Digital twin, Particle breakage, Nanoindentation, Population balance model, Model validation
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要