Thermal conductivity of spark plasma sintered SiC ceramics with Alumina and Yttria

Journal of the European Ceramic Society(2021)

引用 18|浏览3
暂无评分
摘要
In this study, dense SiC ceramics were fabricated at 1650−1750 °C for 10−60 min by spark plasma sintering (SPS) using 3−10 wt.% Al2O3-Y2O3 as sintering additives. Effects of sintering temperature, sintering additive content and holding time on microstructure as well as correlations between microstructure and thermal conductivity were investigated. An increase in the sintering temperature promotes grain growth. Extending holding time has little influence on grain size but results in formation of continuous network of sintering additive, which increases interfacial thermal resistance and thus decreases thermal conductivity. For SiC ceramics composed of continuous SiC matrix and discrete secondary phase (yttrium aluminum garnet, YAG), an increase in the sintering additive content results in smaller grain size and lower thermal conductivity. The lower thermal conductivity of the SiC ceramic with higher sintering additive content is mainly due to the smaller grain size rather than the low intrinsic thermal conductivity of YAG.
更多
查看译文
关键词
SiC,SPS,Interfacial thermal resistance,Grain size,Thermal conductivity
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要