Phosphorus and uranium are both vital elements for society. In recent decades, fears have arisen about the future availability of low-cost phosphorus and uranium. This has resulted in pressure to de-centralize production of both elements by utilizing lower-grade or complex deposits. The research presented here focused on phosphorus-containing apatite ores with uranium impurities; in order to separate uranium by selective and sequential bioleaching before phosphorus leaching. This would create an alternative process route for solvent-extraction, used to remove/recover uranium from the phosphorus acid product of apatite H2SO4 wet process. In this work, it was seen that the used fluorapatite ore required 24 h leaching at pH 1 by H2SO4 to result in 100% leaching yield for phosphorus. As this ore did not contain much uranium, an artificial fluorapatite-uranium ore was prepared by mixing standard uranium ore and fluorapatite. The research with this ore showed that 89% of uranium dissolved in 3 days at pH > 2 and leaching was improved by applying Fe3+ oxidant. In these conditions only 4% of phosphorus was leached. By prolonged (28 days) leaching 95% uranium yield was reached. According to the experiments, the iron in the uranium leach solution would be mainly Fe3+, which allows the use of H2O2 for uranium recovery and then direct use of spent leachate for another uranium leaching cycle. After the dissolution of uranium, 90% of phosphorus was dissolved by decreasing the pH to 1.3. This was done by bioleaching, by utilizing biogenic sulfur oxidation to sulfuric acid.
更多
查看译文
关键词
bioleaching,phosphorus,fluorapatite,uranium
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要