The effect of high-pressure gaseous H2 on the fracture behavior of pipeline steel X70 and austenitic stainless steel type 304L and 316L was investigated by means of notched-tensile tests at 10 MPa H2 gas and various test speed. The notch tensile strength of pipeline X70 steel and austenitic stainless steels were degraded by gaseous H2, and the deterioration was accompanied by noticeable changes in fracture morphology. The loss of notch tensile strength of type 316L and X70 steels was comparable, but type 304L was more susceptible to hydrogen embrittlement than the others. In the X70 steel, hydrogen embrittlement increased as test speed decreased until the test speed reached 1.2 × 10−3 mm/s, but the effect of test speed was not significant in 304L and 316L steels.
更多
查看译文
关键词
Fracture morphology,Hydrogen embrittlement,Strain rate effect,Notched-tensile properties,Hydrogen absorption,Martensitic transformation
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要