Carbonisation of wood residue into charcoal during low temperature process

Renewable Energy(2016)

引用 65|浏览2
暂无评分
摘要
Torrefaction process of wood residue was tested at 230 °C, 260 °C and 290 °C temperatures under 0.5 h, 1.0 h and 1.5 h time in an electrical furnace. The studied material was characterised in terms of its proximate and ultimate analysis. HHV before and after torrefaction was calculated. The behaviour of raw and torrefied biomass was moreover investigated by thermogravimetric analysis, (TG, DTG) and the structural shrinkage was studied by SEM, too. It was found that the most efficient carbonising process among the tested samples is the process operated under 260 °C and 1.0 h time of heating. The results confirmed the great advantages of torrefied material (charcoal) in contrast to raw biomass. Torrefied biomass has been processed successfully, because torrefied biomass has a higher calorific value and energy density, a lower O/C ratio and moisture content, and is easier to grind and has hydrophobic character. The difference in energy yields has shown lower values at the higher torrefaction temperatures.
更多
查看译文
关键词
Wood biomass,Carbonization,Torrefaction process,Thermogravimetry analysis
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要