Full-Field Microstructure Modeling During Forging a Polycrystalline Γ-Γ′ Nickel-Based Superalloy

Chi-Toan Nguyen,Daniel Galy,Jean-Michel Franchet,Jerome Blaizot,Christian Dumont, Lucie Le Sache, Julien De Jaeger,Baptiste Flipon, Nathalie Bozzolo,Marc Bernacki

SUPERALLOYS 2024, ISS 2024(2024)

引用 0|浏览3
关键词
Rene 65,gamma/gamma ' nickel-based superalloys,Full-field modeling,DIGIMU (R),Microstructure,Recrystallization