Ultrastrong and Ductile Superalloy Joints Bonded with a Novel Composite Interlayer Modified by High Entropy Alloy

L. Yuan, F. Y. Jiang, D. Hao, Y. Z. Yang,T. H. Chou,J. X. Zhang, J. Gan, J. L. Li,J. T. Xiong,T. Yang

JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY(2025)

Cited 0|Views4
Key words
Multi-interlayer composite bonding,High entropy alloy,FGH98 superalloy,Microstructure,Plastic deformation behavior