Atomic-Layer Deposition of the Single-Atom Pt Catalyst on Vertical Graphene for H2 Sensing

ACS APPLIED NANO MATERIALS(2024)

Cited 0|Views10
Key words
single-atom catalyst,vertical graphene,atomic-layerdeposition,platinum,hydrogen sensor