Microstructure and Mechanical Properties of GH4169D Superalloy Fabricated by Hybrid Arc and Micro-Rolling Additive Manufacturing

ACTA METALLURGICA SINICA(2024)

Cited 0|Views10
Key words
additive manufacturing,arc and micro-rolling,GH4169D superalloy,heat treatment,microstructure,mechanical property