Improved Tensile Properties of Selective Laser Melted GH4099 Superalloy Assisted by Appreciable Work Hardening Ability
Materials Characterization(2024)
Key words
Ni -based alloys,Selective laser melting,Tensile property,Work hardening ability,Microstructure,Small punch test