Atomic layer deposition niobium oxide and lithium niobium oxide as a protection technique for anode-free batteries
BATTERY ENERGY(2024)
摘要
As demand for extended range in electric vehicles and longer battery lifetimes in consumer electronics has grown, so have the requirements for higher energy densities and longer cycle lifetimes of the cells that power them. One solution to this is the implementation of an "anode-free" battery. By removing the anode and plating lithium directly onto the current collector, it is possible to access the same capacities and voltage windows as traditional lithium metal batteries, with the entirety of the lithium source coming from the cathode. Herein, a copper foil current collector coated with niobium oxide or lithium niobium oxide through atomic layer deposition (ALD) is applied to extend the cycling life of the anode-free batteries by reducing dendrite formation and improving the stability of the lithium metal surface throughout cycling. The ALD coatings are able to extend the cycle lifetime in full coin cells from 20 cycles to 80% capacity retained in the bare copper controls to 50 and 115 cycles for the NbO and LiNbO coatings, respectively. Over the lifetime of the cells, the ALD-LiNbO is able to cumulatively offer a staggering improvement of an additional 100 kWh L-1 compared to the bare copper control. As demand for extended range in electric vehicles and longer battery lifetimes in consumer electronics has grown, so have the requirements for higher energy densities and longer cycle lifetimes of the cells that power them. One solution to this is the implementation of an "anode-free" battery. By removing the anode and plating lithium directly onto the current collector, it is possible to access the same capacities and voltage windows as traditional lithium metal batteries, with the entirety of the lithium source coming from the cathode. Herein, a copper foil current collector coated with niobium oxide or lithium niobium oxide through atomic layer deposition (ALD) is applied to extend the cycling life of the anode-free batteries by reducing dendrite formation and improving the stability of the lithium metal surface throughout cycling. The ALD coatings are able to extend the cycle lifetime in full coin cells from 20 cycles to 80% capacity retained in the bare copper controls, to 50 and 115 cycles for the NbO and LiNbO coatings, respectively. Over the lifetime of the cells, the ALD-LiNbO is able to cumulatively offer a staggering improvement of an additional 100 kWh L-1 compared to the bare copper control.image
更多查看译文
关键词
anode-free,atomic layer deposition,lithium ion battery,thin films
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要