We report on the excitonic transition energy E0 and spin–orbit split-off energy Δ0 of γ-AgxCu1–xI alloy thin films studied by using reflectivity measurements at temperatures between 20 K and 290 K. The observed bowing behavior of the E0 transition as a function of the alloy composition is explained based on first-principles band structure calculations in terms of different physical and chemical contributions within the description of ordered alloys. The spin–orbit coupling is found to increase from a value of 640 meV for CuI to approximately 790 meV for AgI. Furthermore, we show that the temperature-dependent bandgap shift between 20 K and 290 K decreases with increasing Ag-content from 25 meV for CuI to 6 meV for AgI. We attribute this behavior mostly to changes in the contribution of thermal lattice expansion to the bandgap shift.
更多
查看译文
关键词
optical properties,thin films,ag<i>x</i>cu1–<i>x</i>i,alloy
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要