Low‐cycle Fatigue Life Prediction of Powder Metallurgy Superalloy Considering Characteristic Parameters of Inclusions

FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES(2024)

Cited 1|Views16
Key words
characteristic parameters of inclusions,fatigue life prediction model,low-cycle fatigue,non-metallic inclusions,powder metallurgy superalloy