The Synergistic Effect of Trace Ag and Hot Extruding on the Microstructure and Properties of a Biodegradable Mg-Zn-Sr-Ag Alloy.

Materials (Basel, Switzerland)(2023)

引用 0|浏览2
暂无评分
摘要
To further improve the mechanical properties and corrosion resistance of the biodegradable magnesium (Mg) alloy, the Mg-4Zn-0.5Sr-xAg alloy (x = 0.2 wt.%, 0.5 wt.%, 1.0 wt.%, and 2.0 wt.%) was smelted in vacuum under the protection of inert gas. The effect of the Ag content on the microstructure and mechanical properties of Mg-4Zn-0.5Sr was tested. The results show that the comprehensive properties of Mg-4Zn-0.5Sr-0.5Ag are best. The grain size of the Mg-4Zn-0.5Sr-0.5Ag alloy is minimal, that is, 83.28 μm. The average tensile strength (σ), yield strength (σ), elongation (ε), and hardness for the Mg-4Zn-0.5Sr-0.5Ag alloy is 168.00 MPa, 88.00 MPa, 12.20%, and 59.90 HV, respectively. To further improve the properties of cast Mg-4Zn-0.5Sr-0.5Ag alloy, extruding treatment was conducted. After extrusion deformation, the grain size of the alloy was significantly refined to 9 μm; at the same time, fine second phases were formed and evenly distributed in the matrix. And then, the mechanical properties of the alloy are significantly enhanced due to the effect of fine crystal strengthening and dispersion strengthening. The σ, σ, ε, and hardness value for the extruded Mg-4Zn-0.5Sr-0.5Ag alloy are 236.00 MPa, 212.00 MPa, 18.97%, and 65.42 HV, respectively. Under the synergistic action of adding the Ag element and extrusion treatment, the grain size of the alloy was significantly refined and the coarse second phase in the alloy became refined to disperse in the matrix, which benefits the formation of electric couples characterized as small cathode-large anode between the second phase and Mg matrix. During full immersion, corrosion products covered on the large anode surface could reduce the galvanic corrosion tendency.
更多
查看译文
关键词
alloy,trace ag,mg-zn-sr-ag
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要