Area-Selective Atomic Layer Deposition for Resistive Random-Access Memory Devices.
ACS applied materials & interfaces(2023)
摘要
Resistive random-access memory (RRAM) is a promising technology for data storage and neuromorphic computing; however, cycle-to-cycle and device-to-device variability limits its widespread adoption and high-volume manufacturability. Improving the structural accuracy of RRAM devices during fabrication can reduce these variabilities by minimizing the filamentary randomness within a device. Here, we studied area-selective atomic layer deposition (AS-ALD) of the HfO dielectric for the fabrication of RRAM devices with higher reliability and accuracy. Without requiring photolithography, first we demonstrated ALD of HfO patterns uniformly and selectively on Pt bottom electrodes for RRAM but not on the underlying SiO/Si substrate. RRAM devices fabricated using AS-ALD showed significantly narrower operating voltage range (2.6 × improvement) and resistance states than control devices without AS-ALD, improving the overall reliability of RRAM. Irrespective of device size (1 × 1, 2 × 2, and 5 × 5 μm), we observed similar improvement, which is an inherent outcome of the AS-ALD technique. Our demonstration of AS-ALD for improved RRAM devices could further encourage the adoption of such techniques for other data storage technologies, including phase-change, magnetic, and ferroelectric RAM.
更多查看译文
关键词
area-selective atomic layer deposition, dielectrics, resistive random-access memory, filament confinement, data storage device
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要