Synthesis of Micron-Sized WS2 Crystallites Using Atomic Layer Deposition and Sulfur AnnealingKamesh Mullapudi,Rafik Addou,Charles. L. Dezelah,Daniel F. Moser,Ravindra K. Kanjolia,Jacob H. Woodruff,John. F. Conley JrCHEMISTRY OF MATERIALS(2023)引用 6|浏览14关键词Two-Dimensional MaterialsAI 理解论文溯源树样例生成溯源树,研究论文发展脉络Chat Paper正在生成论文摘要