Atomic layer deposition of ?-Al2O3 from trimethylaluminum and H2O: Effect of process parameters and plasma excitation on structure development
JOURNAL OF CRYSTAL GROWTH(2023)
摘要
Aluminum oxide (Al2O3) thin films were deposited from trimethylaluminum (TMA) and H2O on Si substrates and alpha-Cr2O3 seed layers using thermal and plasma-assisted atomic layer deposition (ALD). All films deposited on Si were amorphous. On the alpha-Cr2O3 seed layers, alpha-Al2O3 was formed at temperatures >= 350 degrees C in the thermal ALD and at >= 325 degrees C in the plasma-assisted ALD processes. The Ar plasma used in the experiments most significantly contributed to crystallization when applied during the purge period following the H2O pulse or during the H2O pulse and the following purge. Application of plasma during the TMA pulse, during the purge following the TMA pulse, or only during the H2O pulse suppressed the crystal growth and could potentially be applied as a crystal growth inhibitor.
更多查看译文
关键词
A1, Crystal structure, Surface processes, A3, Atomic layer epitaxy, Plasma-assisted deposition, B1, Aluminum oxide, B2, Dielectric materials
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要