The initiation of internal fatigue cracks in very high cycle fatigue of Ti-6Al-4V alloy was investigated using synchrotron radiation X-ray computed tomography (SR-CT). Micro-CT detected 28 cracks that were distributed across the examined volume of CYRILLIC CAPITAL LETTER EF1.8 x L 2.5 mm. No apparent correlation was observed between the spatial distribution, initial lengths, and initiation lives of cracks. The crack growth rate of the facet-sized crack varied widely; some cracks propagated rapidly, whereas no crack growth was observed for other cracks over a specific period of time after detection. Using nano-CT, the several grain-sized internal cracks and their microstructures were clearly and nondestructively visualized. In the field of view, many primary alpha phases were detected; however, no other cracks were observed. The multiple facet initiation site, which is commonly observed for titanium alloys, might not be due to the concurrently initiated facets but may be caused by the small crack growth accompanied by facet formation.
更多
查看译文
关键词
computed tomography,gigacycle fatigue,internal fatigue crack,nondestructive inspection,synchrotron radiation light,titanium alloy
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要