Significance of Melt Pool Structure on the Hydrogen Embrittlement Behavior of a Selective Laser-Melted 316L Austenitic Stainless Steel.

Materials (Basel, Switzerland)(2023)

引用 2|浏览24
暂无评分
摘要
The hydrogen embrittlement (HE) behavior of a selective laser-melted (SLM) 316L austenitic stainless steel has been investigated by hydrogen charging experiments and slow strain rate tensile tests (SSRTs) at room temperature. The results revealed that compared to the samples without H, the ultimate tensile strength (UTS) and elongation (EL) of specimens were decreased from 572 MPa to 552 MPa and from 60% to 36%, respectively, after 4 h of electrochemical hydrogenation with a current density of 100 mA/cm. The negative effects of hydrogen charging were more pronounced on the samples' ductility than on their strength. A quasi in situ EBSD observation proved that there was little phase transformation in the samples but an increased density of low angle grain boundaries, after 4 h H charging. After strain was applied, the surface of the H-sample displayed many hydrogen-induced cracks along the melt pool boundaries (MPBs) showing that these MPBs were the preferred areas for the gathering and transferring of hydrogen.
更多
查看译文
关键词
austenitic stainless steel,hydrogen embrittlement,mechanical properties,quasi in situ EBSD,selective laser melting
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要