Mechanical Performance, Structure and Fractography of ABS Manufactured by the Fused Filament Fabrication Additive Manufacturing
Annals of "Dunarea de Jos" University of Galati, Fascicle XII, Welding Equipment and Technology(2022)
Key words
abs polymer,additive manufacturing,fused filament fabrication,mechanical properties,three-point bend test,fractography and structure visualization