Nanoindentation study of the viscoelastic properties of human triple negative breast cancer tissues: Implications for mechanical biomarkers.
Acta biomaterialia(2023)
摘要
This paper presents the results of a combined experimental and theoretical study of the structure and viscoelastic properties of human non-tumorigenic mammary breast tissues and triple negative breast cancer (TNBC) tissues of different histological grades. A combination of immunofluorescence and confocal microscopy, and atomic force microscopy is used to study the actin cytoskeletal structures of non-tumorigenic and tumorigenic breast tissues (grade I to grade III). A combination of nanoindentation and statistical techniques is then used to measure viscoelastic properties of non-tumorigenic and human TNBC of different histological grades. A Standard Fluid Model/Anti-Zener Model II is also used to characterize the viscoelastic properties of the non-tumorigenic and tumorigenic TNBC tissues of different grades. The implications of the results are discussed for the potential application of nanoindentation and statistical deconvolution techniques to the development of mechanical biomarkers for TNBC detection/cancer diagnosis. STATEMENT OF SIGNIFICANCE: There is increasing interest in the development of mechanical biomarkers for cancer diagnosis. Here, we show that nanoindentation techniques can be used to characterize the viscoelastic properties of normal breast tissue and TNBC tissues of different histological grades. The Standard Fluid Model (Anti-Zener Model II) is used to classify the viscoelastic properties of breast tissues of different TNBC histological grades. Our results suggest that breast tissue and TNBC tissue viscoelastic properties can be used as mechanical biomarkers for the detection of TNBC at different stages.
更多查看译文
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要