Atomic layer deposition of Zr-sandwiched ZnO thin films for transparent thermoelectrics.
Nanotechnology(2022)
摘要
Atomic layer deposited (ALD) transparent thermoelectric materials enable the introduction of energy harvesting and sensing devices onto surfaces of various shapes and sizes in imperceptible manner. Amongst these materials, ZnO has shown promising results in terms of both thermoelectric and optical characteristics. The thermoelectric performance of ZnO can be further optimized by introducing extrinsic doping, to the realization of which ALD provides excellent control. Here, we explore the effects of sandwiching of ZrOlayers with ZnO on glass substrates. The room-temperature thermoelectric power factor is maximised at 116μW mKwith samples containing a 2% nominal percentage of ZrO. The addition of ZrOlayers is further shown to reduce the thermal conductivity, resulting in a 20.2% decrease from the undoped ZnO at 2% doping. Our results contribute to increasing the understanding of the effects of Zr inclusion in structural properties and growth of ALD ZnO, as well as the thermal and thermoelectric properties of Zr-doped ZnO films in general.
更多查看译文
关键词
atomic layer deposition,thermoelectric,transparent,zinc oxide,zirconium
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要