Dislocations mobility in superalloy-steel hybrid components produced using wire arc additive manufacturing
Materials & Design(2022)
摘要
•Inconel 718/Steel S275 hybrid component produced by WAAM.•Integrated interface in all various states of as-built, solutionized, and aged.•Bulk texture analyses of WAAM-deposited part using neutron diffraction technique.•Elastic-field mathematical model predicts the dislocations’ mobility and dissociation.•Effect of heat treatment on Peierls-Nabarro stress of perfect and partial dislocations.
更多查看译文
关键词
Wire arc additive manufacturing (WAAM),Inconel 718,Nickel-based superalloys,Interface,Peierls-Nabarro stress