Protecting catalyst active sites with atomic layer deposition: Overcoating formation on a porous heterogeneous catalyst and the effect on catalyst reaction performance

Physical Chemistry Chemical Physics(2022)

引用 0|浏览5
暂无评分
摘要
Atomic layer deposition (ALD) was used to deposit protective overcoating (Al2O3) on an industrially relevant Co-based Fischer-Tropsch catalyst. A trimethylaluminium/water (TMA/H2O) ALD process was used to prepare ~0.7 – 2.2...