High temperature nanoindentation of iron: Experimental and computational study
Journal of Nuclear Materials(2022)
摘要
•Nanoindentation is simulated based on the tensile deformation data.•Dislocation density pattern under the indent analyzed by TEM.•CPFEM simulations agree well with nanoindentation.
更多查看译文
关键词
High temperature,Nanoindentation,CPFEM,Iron