Effect of steel fiber-volume fraction and distribution on flexural behavior of Ultra-high performance fiber reinforced concrete by digital image correlation technique

CONSTRUCTION AND BUILDING MATERIALS(2022)

引用 18|浏览3
暂无评分
摘要
This paper investigated the effect of steel fiber-volume fraction (0.5%, 1.0%, 1.5%, and 2.0%) and distribution on the flexural behavior of ultra-high performance fiber reinforced concrete (UHPFRC). Digital image correlation (DIC) was used to obtain the crack propagation behavior of UHPFRC under bending load. With increasing fiber-volume fraction, the crack-propagation path becomes more zigzagged. Based on the flexural response of UHPFRC and fiber distribution on the crack plane, a correlation between fiber distribution characteristics and flexural behavior was discussed. The fibers number per unit area for S0.5, S1.0, S1.5, and S2.0 were 7, 14, 21, and 31, respectively. The fiber pull-out length in cracked zone with different fiber-volume fractions was about 3.56 mm. The fiber orientation factor (eta(theta)) of S0.5, S1.0, S1.5, and S2.0 were 0.80, 0.79, 0.69 and 0.61 respectively. A quadratic relationship between the eta(theta) and the fiber pull-out number is proposed. The flexural-tensile strength ratio (beta) is about 2.52 for UHPFRC exhibiting deflection hardening behavior. Finally, the post-cracking tensile behavior of UHPFRC was analyzed based on the matrix softening and fiber bridging curve models by the inverse analysis method. The tension softening curves obtained from the tri-linear softening curve analysis exhibited good agreement with the experimental results.
更多
查看译文
关键词
Ultra-high performance fiber reinforced concrete, Steel fiber-volume fraction, Fiber distribution, Flexural behavior, Digital image correlation
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要