Morphological characterization of semi-crystalline POM using nanoindentation
International Journal of Polymer Analysis and Characterization(2021)
摘要
Nanoindentation (NI) is a contact method to investigate localized micromechanical properties of materials, whereby NI of semi-crystalline polymers is challenging. The influence of morphological structures such as spherulites or crystal-lamellae on localized NI depth-force behavior is discussed controversially in literature. Hence, the main objective of this study is to determine the influence of crystalline zones on NI results.
更多查看译文
关键词
Nanoindentation,polyoxymethylene,semi-crystalline polymer,creep,atomic force microscopy