Surface Versus Bulk Defect-Related Properties Of The Wustite Phase (Feo) In Gas/Solid Equilibrium

ACS APPLIED ENERGY MATERIALS(2020)

引用 2|浏览2
暂无评分
摘要
This work determined isothermal work function (WF) changes as a function of oxygen activity, p(O-2), for the Fe-O-2 system within the stability range of the FeO phase at elevated temperatures (948 K-1223 K). The slope of the WF changes versus log p(O-2), which represents a defect-related quantity for the surface layer, mo, is compared with a similar defect-related factor for the bulk phase of FeO. The plot of the ma, factor as a function of temperature indicates that long-range interactions between defects within the surface layer result in the formation of a low-dimensional quasi-isolated surface structure (QISS) that resembles the structures already observed for other metal oxides, such as NiO, CoO, and ZrO2. The interactions between defects within the QISS increase with the decrease of temperature. The proposed theoretical model considers the effect of segregation of intrinsic defects on surface composition in terms of the iron-to-oxygen ratio. Derivation of a specific defect disorder for the outer surface layer requires determination of the local crystalline structure of the QISS.
更多
查看译文
关键词
iron oxide, defect disorder, surface layer, work function, FeO, equilibrium
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要