Process, Microstructure and Microhardness of GH3039 Superalloy Processed by Laser Metal Wire Deposition
JOURNAL OF ALLOYS AND COMPOUNDS(2021)
关键词
Laser metal deposition,GH3039 superalloy,Geometrical characteristics,Microstructure,Microhardness