Comprehensive Investigation Of The Viscoelastic Properties Of Pmma By Nanoindentation
POLYMER TESTING(2021)
摘要
Instrumented nanoindentation (NI) was used to examine the viscoelastic properties of poly(methyl methacrylate) (PMMA) as an amorphous polymer model. An evaluation combining adhesive contact and empiric spring-dashpot models has been applied to obtain the instantaneous elastic modulus E-0 and the infinitely elastic modulus E-infinity from nanoindentation creep curves. The value of E-0 has been compared to moduli obtained with atomic force microscopy-based nanoindentation (AFM-NI) and compression tests. Furthermore, the elastic modulus has been evaluated by the method introduced by Oliver and Pharr (O&P) for the NI and AFM-NI results. Comparison of the elastic modulus E-0 from the creep measurements of NI and AFM-NI to compression tests reveals good agreement of the results. However, only the O&P based AFM-NI results yield to lower values.
更多查看译文
关键词
Nanoindentation, Amorphous, Creep, AFM, Compression test
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要