Plasma-wall interactions at the first wall in fusion experimental devices are critical for the life time of plasma facing components and tokamak operation. In-situ measurements of these plasma-wall interaction processes are required in long pulse devices in order to understand better the underlying mechanisms as well as monitoring of the tritium content of the first wall as an immediate safety application. In this work we present measurements of the deuterium retention in the first wall of EAST using laser-induced ablation spectroscopy. The diagnostic is applied during plasma operation and the dynamic retention for graphite and tungsten as plasma-facing materials are compared, showing more than three times higher short-term retention in graphite than in tungsten. Laser based analysis is applied during a shift of the vertical positions of the plasma column in limited as well as in the start-up phase of discharges in diverted magnetic configuration. Plasma core densities of n(e) = (1.5-3.2) x 10(19)/m(3) are chosen to vary the ion flux to the first wall and study saturation effects of deuterium on the surface first wall materials during tokamak plasma operation. A linear dependence of the retention from ion fluence is observed for graphite as PFC up to 3 x 10(18)D(+)/cm(2), followed by a constant retention up to fluences of 3.5 x 10(19)D(+)/cm(2) for nearby first wall temperatures of T-PFC approximate to 350 K.
更多
查看译文
关键词
Laser-induced ablation spectroscopy, Plasma-facing components, Deuterium retention, In situ analysis, EAST tokamak
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要