Na0.5Bi0.5TiO3-0.06BaTiO(3) relaxor ferroelectrics ceramic samples doped with 1 wt% of CuO, Fe2O3, Sb2O3, La2O3 and Ta2O5 were investigated by means of dielectric and acoustic emission methods in the high-temperature range. Dielectric constants exhibited a wide and smeared maximum at the temperature T-m, accompanied by acoustic emission sharp bursts, but the dielectric constants exhibited no anomaly when further transiting into cubic paraelectric phase at the temperature T-p, accompanied by acoustic emission sharp bursts, too. Based on acoustic emission data the shifts of these two temperatures, T-m and T-p, in dependence on a wt% of the incorporated ions as well as the acoustic emission count rate distribution in dependence on the incorporated ions radii were plotted and discussed.
更多
查看译文
关键词
77,80,Jk,77,80,B-,43,40,Le
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要