Chiral mesoporous silica synthesized by a facile strategy for loading and releasing poorly water-soluble drug.

DRUG DEVELOPMENT AND INDUSTRIAL PHARMACY(2020)

引用 2|浏览1
暂无评分
摘要
Most of the mesoporous chiral mesoporous silica (CMS) was synthesized by the chiral surfactant-directing method. In this study, a facile method was designed to synthesize CMS. In this method, achiral amphiphile was used as templating agents, and dilute ammonia solution was applied to induce the chirality of the CMS. Meanwhile, its morphology can be controlled by changing the concentration of the aqueous ammonia solution. The obtained CMS was characterized by dynamic light scattering (DLS), X-ray diffraction (XRD), transmission electron microscopy (TEM), and scanning electron microscopy (SEM). The results showed that all of the CMS possessed highly ordered mesostructures, and as the concentration of ammonia decreases, the chirality of the CMS becomes more obvious. Water-insoluble drug curcumin (Cur) was used as a model drug. The characteristics of CMS before and after drug loading were further detected by Fourier transform infrared spectrometer (FT-IR), N(2)adsorption-desorption and differential scanning calorimetry (DSC). The result showed that Cur was successfully loaded inside the pores of the CMS and remained an amorphous state due to steric inhibition. Additionally, CMS could significantly increase the release rate of Cur under different pH conditions.
更多
查看译文
关键词
Mesoporous silica,chirality,curcumin,ammonia solution,dissolution rate
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要