This study presents the effects of silicon (Si) and manganese (Mn) concentration and of heating rate on the ferrite recrystallization kinetics in seven model alloys with different Si and Mn concentrations, which are of relevance for the development of Advanced High Strength Steels (AHSS). The recrystallization kinetics were studied with in-situ 2D X-ray Diffraction (2D-XRD) and ex-situ microstructure observations using Scanning Electron Microscopy (SEM). The experimentally observed differences in the recrystallization start temperature (T-s), dependent on the Si and Mn concentrations and the heating rate, can be described by combining the non-isothermal JMAK-model with a modified version of Cahn's solute drag model. The modified Cahn model takes into account in an approximate manner that the interaction energy of the solute atoms with the grain boundary depends on the Si and Mn concentrations in the boundary and the Wagner interaction parameters. The collective contribution of the Si and Mn atoms to the increase in the T-s with respect to the reference alloy (without Si and with very little Mn) is higher than would be expected from the simple addition of the effects of the Si and Mn concentrations alone. This means that the interaction between Si and Mn atoms leads to an additional increase in T-s, i.e. a coupled solute drag effect. For the later stages of recrystallization, we have studied the change in the number density and the growth rates of the recrystallizing grains using SEM. The observations show non-random nucleation, early impingement of the grains in the normal-direction and non-constant growth rates of recrystallizing grains.
更多
查看译文
关键词
ferrite recrystallization, recrystallization start temperature, coupled solute drag, manganese, silicon
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要