45-Degree Rafting in Ni-based Superalloys: A Combined Phase-Field and Strain Gradient Crystal Plasticity Study

International Journal of Plasticity(2020)

Cited 43|Views21
Key words
Superalloys,Dislocations,Rafting,Directional coarsening,Phase field,Crystal plasticity