A Fem Multiscale Homogenization Procedure Using Nanoindentation For High Performance Concrete
JOURNAL OF APPLIED AND COMPUTATIONAL MECHANICS(2020)
摘要
This paper aims to develop a numerical multiscale homogenization method for prediction of elastoviscoplastic properties of a high performance concrete (HPC). The homogenization procedure is separated into two-levels according to the microstructure of the HPC: the mortar or matrix level and the concrete level. The elasto-viscoplastic behavior of individual microstructural phases of the matrix are identified from nanoindentation data using an inverse identification method. The micromechanical results are then used as input parameters for numerical elasto-viscoplastic homogenization at microscale. The mortar level is analyzed with numerical homogenization by using the finite element simulation to predict the overall elastoviscoplastic properties of HPC. The results are compared with macroscopic experimental and analytical results from the literature showing a good agreement.
更多查看译文
关键词
Homogenization, Nanoindentation, Finite element simulation, Elasto-viscoplastic model, Multiscale modeling, High performance concrete
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要