Atom site preference and γ′/γ mismatch strain in NiAlCoTi superalloys
Intermetallics(2016)
摘要
The structure and chemistry of NiCoAlTi quaternary superalloys are investigated at the microstructural and atomic scale. Atom probe tomograghy (APT) is used to quantify phase compositions and elemental partitioning behavior. Using aberration corrected electron microscopy, the site occupancy of the atoms within the A3 B structure (L12–type) γ′ phase is determined via atomic resolution energy dispersive X-ray spectroscopy (EDX). Ni is observed to preferentially occupy the A sub-lattice positions for all alloys, while Al and Ti occupy the B sub-lattice. In contrast, Co's site preference changes from a random distribution to the A sub-lattice as the alloy composition changes, in agreement with theoretical predictions from literature. Finally, the lattice strain across the γ′/γ interfaces is measured as a function of alloy composition.
更多查看译文
关键词
Scanning transmission electron microscopy,Quaternary superalloy,Site preference,Strain measurement
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要