Heat capacity by differential scanning calorimetry and thermodynamic functions of BaCe 0.8 Gd 0.1 Y 0.1 O 2.9 in the temperature range of 166–790 K
Journal of Thermal Analysis and Calorimetry(2018)
摘要
In the present study, the heat capacities of barium cerate doped by gadolinium and yttrium oxides were measured for the first time in the temperature range of 166–790 K. The differential scanning calorimeter was used for investigation. There was reproducible anomaly with maximum at 601 K and minimum at 679 K. The experimental results were used to calculate the thermodynamic functions: smoothed heat capacities, enthalpy increment ( H m o ( T ) − H m o (298.15)), and entropy ( S m o ( T )). The heat capacity in the temperature range of 166–602 K was described by a polynomial of the form: C p,m o ( T ) = 83.140 + 0.14943 T − 1.1537 × 10 −4 T 2 − 3.6358 × 10 5 / T 2 (J mol −1 K −1 ). Heat capacity of BaCe 0.8 Y 0.1 Gd 0.1 O 2.9 in the temperature range of 602–680 K was described by a polynomial: C p,m o ( T ) = − 118.18 + 0.71961 T − 5.5387 × 10 −4 T 2 + 5.6948 × 10 +6 / T 2 (J mol −1 K −1 ). The heat capacity in the temperature range of 680–790 K was well described by the equation: C p,m o ( T ) = 1987.1 − 6.9263 T + 8.3407 × 10 −3 T 2 − 3.1992 × 10 −6 T 3 (J mol −1 K −1 ).
更多查看译文
关键词
Doped barium cerate,Heat capacity,DSC
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要