The effect of aging on thermomechanical and metal extraction properties of poly (vinyl chloride)/Aliquat 336 polymer inclusion membranes

DESALINATION AND WATER TREATMENT(2016)

引用 4|浏览2
暂无评分
摘要
The impact of aging PVC/Aliquat 336 polymer inclusion membranes (PIMs) on their thermomechanical properties and heavy metal extraction performance was investigated. The results show that freshly prepared PIMs contain residual tetrahydrofuran (THF) which was used as the solvent for membrane manufacture. Removal of some residual THF by membrane aging resulted in notable changes in the thermomechanical properties of the PIMs. By aging the membrane for 1week at 40 degrees C, the glass transition increased from 42 to 55 degrees C. In addition, while the melting temperature (T-m) of the Aliquat 336 component could not be determined for freshly prepared PIMs, the aged membrane showed a clear T-m value of -19 degrees C. Metal extraction capacity was not affected by membrane aging.
更多
查看译文
关键词
Polymer inclusion membrane (PIMs),Membrane aging,Metal extraction,Poly (vinyl chloride) (PVC),Aliquat 336
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要