Modeling Nonlinear Plasticity Of Bone Mineral From Nanoindentation Data
MULTISCALE SIMULATIONS AND MECHANICS OF BIOLOGICAL MATERIALS(2013)
关键词
anisotropy,hydroxyapatite,nanoindentation,single crystal