Ultraviolet light irradiation on pitting corrosion of Cu-based bulk metallic glasses
Journal of Alloys and Compounds(2016)
摘要
We report the observation that UV irradiation substantially improves pitting corrosion resistance of Cu-based bulk metallic glasses. Specifically, two Cu-based bulk metallic glasses in this study showed more stable passive films under UV irradiation than under irradiation-free condition when polarized in 3.5 wt.% NaCl aqueous solution. This finding indicates that Cu-based bulk metallic glasses are promising to serve in high UV irradiation and corrosive environments.
更多查看译文
关键词
Metallic glasses,Corrosion,Scanning electron microscopy