Sr1-xNaxSiO3-0.5x (x = 0.1, 0.2, 0.3, 0.4) is prepared by solid state reaction of stoichiometric mixtures of SrCO3, Na2CO3, and silica powder (air, 1050 °C, 24-96 h).