Atomic Layer Deposition of Tunnel Barriers for Superconducting Tunnel Junctions
Journal of Low Temperature Physics(2014)
摘要
We demonstrate a technique for creating high quality, large area tunnel junction barriers for normal–insulating–superconducting or superconducting–insulating–superconducting tunnel junctions. We use atomic layer deposition and an aluminum wetting layer to form a nanometer scale insulating barrier on gold films. Electronic transport measurements confirm that single-particle electron tunneling is the dominant transport mechanism, and the measured current–voltage curves demonstrate the viability of using these devices as self-calibrated, low temperature thermometers with a wide range of tunable parameters. This work represents a promising first step for superconducting technologies with deposited tunnel junction barriers. The potential for fabricating high performance junction refrigerators is also highlighted.
更多查看译文
关键词
Superconducting tunnel junctions, Atomic layer deposition, Tunnel barriers
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要