Impact of dual beam laser spike annealing parameters on nickel silicide formation characteristics

Advanced Thermal Processing of Semiconductors(2010)

引用 3|浏览18
暂无评分
摘要
Nickel silicide is a common contact material for current generation microelectronic devices. As the technology nodes become smaller, forming the NiSi phase with milli-second or below annealing is an attractive alternative to conventional RTA annealing because of the potential for increased device performance and yield. This paper will discuss the use of a dual beam laser spike annealing (LSA) to form nickel silicide on silicon wafers in the microsecond regime. A detailed evaluation of anneal times (400μs and 800μs) and anneal exposure (100% and 50% stitching, or single and double anneals) was done on 300mm wafers with NiPtSix film (post-RTA1 anneal/100Å). Analytical testing by sheet resistance, CGS, XRD, AES depth profile, AFM, SEM, and ellipsometry was performed on the wafers to examine the effects of anneal times and exposure on phase transition and/or film morphology. A study of the nickel silicide transition curve by sheet resistance vs. temperature shows that there is a higher NiSi damage threshold temperature for single anneal as compared to double anneal. For uniformly annealed full wafers processed at temperatures slightly below the damage threshold, the results confirm: 1) NiSi was formed with negligible or small differences in film structure and, 2) the 100% stitching single annealed wafers show similar process performance in terms of sheet resistance and within wafer uniformity to the 50% stitching double annealed wafers at both 400 and 800μs.
更多
查看译文
关键词
auger electron spectra,x-ray diffraction,atomic force microscopy,ellipsometry,laser beam annealing,nickel compounds,rapid thermal annealing,scanning electron microscopy,solid-state phase transformations,aes depth profile,afm,nisi,rta,sem,xrd,analytical testing,current generation microelectronic device,damage threshold temperature,dual beam laser spike annealing parameter,microsecond regime,nickel silicide formation,nickel silicide transition curve,phase transition,sheet resistance,silicon wafer,time 400 mus,time 800 mus,uniform annealed full wafer processing,nickel,temperature measurement,x ray diffraction,annealing,heating
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要