Fabrication of Oxide/Semiconducting Coaxial Nanotubular Materials Using Atomic Layer Deposition
Materials Science Forum(2004)
摘要
Novel fabrication routes of oxide/semiconducting hybrid nanotubes or coaxial nanocables with 30similar to200 nanometers of radius and similar to10 micrometers of length using atomic layer deposition (ALD) and soluble nano-templates was reported. In order to fabricate the hybrid nanotubes using nanotemplates, which were treated with surface modification using SAMs in order to achieve selective deposition only onto inner wall of the template. Deposition of metal oxide layers (TiO2, ZrO2) conformally and uniformly onto the wall of templates using ALD. To fabricate metal oxide/CdS nanocables or coaxial nanotubes, CdS was deposited onto metal oxide nanotubes by chemical bath deposition. Coaxial nanocables was also 30-200 nm in diameter and 1.10mum in lengths.
更多查看译文
关键词
nanotube,nanotemplate,atomic layer deposition (ALD),self-assembled monolayer,(SAM) and chemical bath deposition (CBD)
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要